Bore pitting in 81mm mortar barrels
Book information
Description
Royal Armament Research and Development Establishment R.A.R.D.E. Memorandum 8/67, 1967. – 21 p.This report gives details of the examination of pitted barrels and concludes that the major cause of pitting is corrosion of the bores by decomposition products of the bomb obturating rings. Provisional trials with Polycarbonate obturating rings are described. It is considered that the use of Polycarbonate rings will eliminate the prime source of bore corrosion, namely chloride contamination, and also may well reduce the incidence of other forms of secondary corrosion.Contents: Introduction. Examination of pitted barrels. Examination Procedure. Barrels ex P & E.E. Pendine. Barrels ex Middle East Land Forces. Barrels at School of Infantry Netheravon. R.A.R.D.E. Firing Trial. Equipment and ammunition. Trial results. Examination of barrels from R.A.R.D.E. trial. Discussion. Conclusions.
Similar books
Таблицы стрельбы 23-мм спаренной установки ЗУ-23 по наземным целям. ТС № 0210
DJVU
Выписка из таблиц стрельбы 120-мм минометов 2Б11, 2С12 для мин ОФ-843Б и 3С9
Автоматика подрыва боеприпаса - Головной взрыватель ГПВ-1. Руководство службы
DJVU
МО СССР. Дополнение к ТО и ИЭ 100-мм противотанковая пушка Т-12, к Руководству службы 100-мм противотанковая пушка Т-12, к Руководству службы 100-мм противотанковая пушка МТ-12, к Руководству службы 100-мм противотанковая пушка МТ-12. 100-мм выстрелы ЗУБМ10 и ЗУБК8
DJVU
МО СССР. Снаряды Артиллерии Военно-Морского Флота. Альбом
Internal ballistics using two different propellant grain form functions
Interior ballistics modeling: extensions to the one-dimensional XKTC code and analytical studies of pressure gradient for lumped parameter codes